The method of reducing corrosion during grate sintering includes the following steps:
(1) Iron-containing raw materials are classified into iron-containing raw materials I and iron-containing raw materials II; The iron-containing raw material I is that the mass percentage content of any K, Na, Cl, S and F is higher than 0.1% or that the total mass percentage content of any two or more kinds of K, Na, Cl, S and F is higher than 0.2%; Iron-containing material II is iron-containing material excluding iron-containing material I;
(2) The iron-containing raw material I is mixed with flux and fossil fuel for granulation. In the process of granulation, active calcium and iron additives are added on the surface of the formed spherules to obtain spherules ①; In addition, iron-containing raw material II is mixed with flux, fossil fuel and ore return for granulation. In the process of granulation, active calcium and iron and polymer mixed additives are added on the surface of the formed pellets to obtain pellet ②;
(3) The pellet (1) and the pellet (2) are successively distributed, ignited and sintered, and the dust particles in the flue gas at different stages of the sintering process are respectively captured; In the cloth process, the pellet (2) is distributed to the platform of the sintering machine, and the pellet (1) is distributed in the middle and upper layer of the sinter layer.
The method classifies iron-containing raw materials with different contents of harmful elements for granulation and layering, so as to effectively control the emission law of ultrafine particles and prevent grate corrosion.