Analysis Of Main Forms And Causes Of Grate Bar Damage

Mar 27, 2024|

Burning toppled off


Phenomenon of furnace burning or installation too loose, individual drop or large area tip. The reason is:


(1) The furnace working environment is bad and stable 200-950 degrees Celsius cycle alternately, ablative oxidation under the action of high temperature


(2) In the process of charging and unloading, the impact of materials on the furnace strip causes stress change and fracture


(3) The heat insulation sleeve and the trolley beam are deformed, and the grate pin is not restored in time, leading to the grate falling


(4) The use cycle of the furnace bar is not replaced in time


(5) furnace processing technology and composition affect the high temperature resistance strength


(6) The process control management system is not perfect and the technical level of operators is defective


Furnace block material paste solid


Phenomenon: mostly bar and heat insulation sets of sticky material, once formed, the more the more sticky, lead to bar and a decrease in heat insulation set play, permeability is a sharp drop in the region, local wet and serious, gradual development led to the bar and heat insulation sleeve with no clearance, the whole car paste stuck out, is a car lose permeability, cannot make sintering process.


After first plugging paste paste plugging process, in the process of sintering, pave base small fraction into hot bar gap if not clear in time, after reaching a certain degree, permeability variation of sintering process is slow, easy to form a wet floor, when wet and serious shop close to the bar and base will be attached on the bar, when heated to burn block forming paste plugging in the end. The reason is:


(1) The influence of raw fuel conditions, resulting in unstable and uneven material composition, poor spherification, fuel volatile ash.


(2) the gap between the grate and the bottom material particle size contradiction, small particle size bottom material plug in the grate gap.


(3) The dust removal ash is not reasonable and unstable.


(4) influence of furnace strip processing technology and composition.


(5) The fluctuation of the feed quantity under the batching causes the fluctuation of the water composition of the mixture.


(6) The technical level of operators and the defects of process control management under different raw material conditions.


(7) The furnace bar heat insulation sleeve is not reasonable, and the activity gap is small.


(8) Improper air volume negative pressure air supply system.


When the furnace is burned, if not handled in time, a small range will cause holes, and a large range will cause falling. In the car began to air leakage into the nose after sealing plate system, material with convulsions into bellows and flue dust ash content increased, the fan rotor and increase system equipment wear and tear, fan current rise, material surface ignition uneven, due to the slow, can't even get to air leakage of sintering process, directly affect the yield and quality of sinter and cost, caused by the factors of vicious circle, Operator labor intensity increases safety risks also increase.