What are the common defects of high chromium cast iron?

Jul 19, 2023|

The common defects of cast iron castings are: pores, sticky sand, sand inclusions, trachoma, sand swelling, cold shut, insufficient pouring, etc.
1. Stomata
The gas does not escape in time before the liquid metal crust, and the hole-like defects are generated in the casting. The inner walls of the stomata are smooth, bright or slightly oxidized. After the pores are generated in the casting, the effective bearing area will be reduced, and stress concentration will be caused around the pores, which will reduce the impact resistance and fatigue resistance of the casting. Pores also reduce the compactness of castings, causing some castings that are required to withstand hydrostatic tests to be scrapped. In addition, pores also have adverse effects on the corrosion resistance and heat resistance of castings.
Prevent the generation of pores: reduce the gas content in the molten metal, increase the air permeability of the sand mold, and add a gas outlet riser at the highest point of the cavity, etc.
2. Sticky sand
A layer of hard-to-remove sand adheres to the surface of the casting called sticky sand. Sticky sand not only affects the appearance of castings, but also increases the workload of casting cleaning and cutting, and even affects the life of the machine
Prevent sticky sand: add coal powder to the molding sand, and apply anti-sticky sand paint on the surface of the mold.
3. Sand inclusion
Grooves and scar defects formed on the surface of castings are very easy to occur when casting thick and large flat castings with wet molds.
Most of the sand inclusions in the casting are in contact with the upper surface of the sand mold. The upper surface of the cavity is affected by the radiant heat of the molten metal, and it is easy to arch and warp. When the warped sand layer is continuously washed by the molten metal flow May break and shatter, stay in place or be carried elsewhere. The larger the upper surface of the casting, the greater the volume expansion of the molding sand and the greater the tendency to form sand inclusions.
4. Trachoma
A cavity-like defect filled with molding sand in or on the casting.
5. Expanding sand
Under the pressure of the molten metal during pouring, the mold wall moves and the casting partially expands to form a defect.
In order to prevent sand swelling, the strength of the sand mold and the rigidity of the sand box should be increased, and the pressure or fastening force of the box should be increased when the box is closed, and the pouring temperature should be appropriately reduced to make the surface of the molten metal crust early, so as to reduce the impact of the molten metal on the mold. pressure
6. Cold insulation and insufficient pouring
The filling capacity of liquid metal is insufficient, or the filling conditions are poor. Before the cavity is filled, the molten metal will stop flowing, which will cause insufficient pouring or cold shut defects in the casting. Insufficient pouring will prevent the casting from obtaining a complete shape; when the casting is cold shut, although the casting can obtain a complete shape, the mechanical properties of the casting are severely damaged due to the presence of incompletely fused joints.
Prevent under pouring and cold shut: increase pouring temperature and pouring speed.