Heat resistant cast steel 1.4823
Mar 12, 2025| 1.4823 is an austenitic stainless steel, renowned for its excellent high-temperature oxidation and corrosion resistance. This material exhibits outstanding comprehensive performance in extreme temperature environments (-253°C to 700°C), particularly demonstrating leading yield strength among similar alloys below 650°C.
Core characteristics
Chemical composition: With chromium (Cr), nickel (Ni), and silicon (Si) as the core alloying elements, the chromium content supports its oxidation resistance, the nickel element enhances high-temperature stability, and the silicon component further improves corrosion resistance.
Corrosion resistance: It can resist the erosion of most strong acids and alkalis, and remains stable in high-temperature sulfur-containing gases and oxidative environments, making it suitable for harsh working conditions such as chemical reactors and flue gas desulfurization devices.
Mechanical properties: The tensile strength reaches 520 - 670 MPa, the yield strength is ≥ 205 MPa, and the elongation is ≥ 40%, combining high hardness and good ductility to meet the structural reliability requirements under dynamic loads.
Process characteristics: It supports conventional welding processes such as TIG and MIG, and no complex heat treatment is required after welding, significantly reducing manufacturing and maintenance costs.
Typical applications
Energy field: Pipeline of nuclear reactor cooling system, high-temperature components of petroleum cracking unit
Aerospace: Fuel delivery pipe of rocket engine, high-temperature seal of turbine
Industrial equipment: Sintering machine grate, lining of chemical reaction kettle, corrosion-resistant components of pharmaceutical equipment
Special environment: Chloride ion corrosion-resistant components of offshore platforms, structural components of acid gas treatment system
Technical points
The surface treatment should adopt pickling and passivation processes to maximize the corrosion resistance potential, and the roughness control is recommended to be Ra ≤ 0.8 μm.
In continuous high-temperature working conditions, it is recommended to control the upper limit of the working temperature below 680°C to ensure the material structure stability.
During cold working, a solution treatment at 1150°C is required to eliminate work hardening and restore the plasticity of the material.
Through optimizing the alloy ratio, this material significantly improves the high-temperature strength and carburization resistance while maintaining the processing advantages of traditional austenitic stainless steel. It has now become the preferred material in high-end equipment manufacturing fields such as petrochemical and nuclear power.